Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 900 Clear Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman 980-05V0 Grey Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D412 |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Tensile Strength | 65.5 MPa @Temperature 23.0 °C, Time 0.000 sec |
9500 psi @Temperature 73.4 °F, Time 0.000 hour |
Sheet Immersion in Diesel Fuel |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Tensile Strength | 65.5 MPa @Temperature 23.0 °C, Time 2.42e+6 sec |
9500 psi @Temperature 73.4 °F, Time 672 hour |
Sheet Immersion in Diesel Fuel |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Ensinger Tecapeek® XP-108 Compression Molded PEEK Compound, 20% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 65.5 - 75.8 MPa | 9500 - 11000 psi | ASTM D638 |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Tensile Strength | 65.5 - 75.8 MPa | 9500 - 11000 psi | ASTM D638 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | |
Atom Adhesives AA-CARB 61 Epoxy Adhesive AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and me.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | Cured |
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | cured |
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value .. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | cured |
Atom Adhesives AA-DUCT 903 Epoxy Adhesive AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha.. |
|||
Tensile Strength | 65.5 - 79.3 MPa | 9500 - 11500 psi | |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Tensile Strength | 65.5 - 79.3 MPa | 9500 - 11500 psi | |
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing .. |
|||
Tensile Strength | 65.5 - 79.3 MPa | 9500 - 11500 psi | |
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ.. |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D638 |
Aaron Industries AAROPRENE® AEN 6600-1 Nylon 6/6 Engineered Resin |
|||
Tensile Strength | 65.5 MPa | 9500 psi | ASTM D412 |
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b.. |
|||
Tensile Strength | 65.5 - 79.3 MPa | 9500 - 11500 psi | |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |