Mechanical Properties Metric English Comments
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Quantum Acetal-Copolymer
Information provided by Quantum Advanced Engineering Plastics
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 900 Clear Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 910 Utility Black Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 910-05V0 Utility Black Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 920 Black Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 930 White Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 930-05V0 White Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 980 Grey Polycarbonate
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman 980-05V0 Grey Polycarbonate Glass Filled
Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc.
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Shuman FR980V0 Grey Polycarbonate Flame Retardant
Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
Tensile Strength 65.5 MPa
9500 psi
ASTM D412
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Tensile Strength 65.5 MPa

@Temperature 23.0 °C,
Time 0.000 sec
9500 psi

@Temperature 73.4 °F,
Time 0.000 hour
Sheet Immersion in Diesel Fuel
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Tensile Strength 65.5 MPa

@Temperature 23.0 °C,
Time 2.42e+6 sec
9500 psi

@Temperature 73.4 °F,
Time 672 hour
Sheet Immersion in Diesel Fuel
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Ensinger Tecapeek® XP-108 Compression Molded PEEK Compound, 20% PTFE Filled
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Tensile Strength 65.5 - 75.8 MPa
9500 - 11000 psi
ASTM D638
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6
NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Tensile Strength 65.5 - 75.8 MPa
9500 - 11000 psi
ASTM D638
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6
NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti..
Tensile Strength 65.5 MPa
9500 psi
Atom Adhesives AA-CARB 61 Epoxy Adhesive
AA-CARB 61 is an epoxy adhesive and coating formulation based on conductive carbon. AA-CARB 61 is recommended for electronic bonding and sealing applications that require both fine electrical and me..
Tensile Strength 65.5 MPa
9500 psi
Cured
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating
AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of..
Tensile Strength 65.5 MPa
9500 psi
cured
Atom Adhesives AA-DUCT 902LP Epoxy Adhesive
AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value ..
Tensile Strength 65.5 MPa
9500 psi
cured
Atom Adhesives AA-DUCT 903 Epoxy Adhesive
AA-DUCT 903 is an epoxy adhesive and coating formulation based on Nickel. This epoxy nickel formulation offers the maximum continuity of conductivity with an electrical resistivity value of less tha..
Tensile Strength 65.5 - 79.3 MPa
9500 - 11500 psi
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie..
Tensile Strength 65.5 - 79.3 MPa
9500 - 11500 psi
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound
BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing ..
Tensile Strength 65.5 - 79.3 MPa
9500 - 11500 psi
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound
BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ..
Tensile Strength 65.5 MPa
9500 psi
ASTM D638
Aaron Industries AAROPRENE® AEN 6600-1 Nylon 6/6 Engineered Resin
Tensile Strength 65.5 MPa
9500 psi
ASTM D412
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane
Features: Excellent physical properties, hydrolysis resistance and improved temperature resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and b..
Tensile Strength 65.5 - 79.3 MPa
9500 - 11500 psi
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound
BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma..