Material Notes:
AA-DUCT 902LP is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of less than 1x10-4 ohm-cm. AA-DUCT 902LP is also characterized by a wide operating temperature range from –50 to +170°C. AA-DUCT 902LP is recommended for electronic bonding and sealing applications that require both fine electrical and mechanical properties.Appearance: SilverCure Type: Heat cure or Room TemperatureBenefits:High strengthPerfect bondCold solder for heat sensitive components Mix Ratio by weight: 100:6/Resin:Hardener Substrates: Excellent choice aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards. Typical Application: Electrical, conductive, rmi/efi shielding, circuitry, printed circuit board and electronics repairInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.79 g/cc
2.79 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
cured
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
cured
Tensile Strength 65.5 MPa
9500 psi
cured
Compressive Strength 96.5 MPa
14000 psi
cured
Shear Strength 64.8 MPa
9400 psi
Lap, cured
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C
8.33 µin/in-°F
Thermal Conductivity 14.4 W/m-K
100 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 170 °C
338 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.00010 ohm-cm
<= 0.00010 ohm-cm
Processing Properties Metric English Comments
Cure Time 2.00 min

@Temperature 120 °C
0.0333 hour

@Temperature 248 °F
5.00 min

@Temperature 100 °C
0.0833 hour

@Temperature 212 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
uncured
Shelf Life 12.0 Month
12.0 Month
uncured
Descriptive Properties Value Comments
Viscosity Paste
uncured