Mechanical Properties Metric English Comments
Tensile Strength 300 - 400 MPa
43500 - 58000 psi
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat..