Latrobe DuraTechâ„¢ M48 Powder Metal High Speed Steel (ASTM M48)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name DuraTech™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe DuraTechâ„¢ M48 Powder Metal High Speed Steel (ASTM M48).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraTech M48 super high speed steel is a high-performance high speed steel which exhibits superior hot (red) hardness compared to T15 and M42 high speed steels, and wear resistance comparable to that of T15. DuraTech M48 can be heat treated to 70 HRC, and the high cobalt content enables the steel to maintain high hardness at elevated service temperatures. Vanadium carbides provide the high wear resistance, and the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure maximize the toughness of the steel. DuraTech M48 offers improved cutting tool life compared to the M-series high speed steels. Typical applications include form tools, broaches, milling cutters, hobs, and any special cutting tool where high hot hardness is required.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 8.26 g/cc
8.26 g/cc
Density 8.25 g/cc
0.298 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 65.5
65.5
Oil Quenched from 1199°C, 3 minutes
67
67
Oil Quenched from 1177°C, 5 minutes
68
68
Oil Quenched from 1149°C, 10 minutes
Modulus of Elasticity 214 GPa
31000 ksi
Machinability 10 - 15 %
10 - 15 %
1% Carbon Steel
Component Elements Properties Metric English Comments
Carbon, C 1.55 %
1.55 %
Chromium, Cr 4.0 %
4.0 %
Cobalt, Co 9.0 %
9.0 %
Iron, Fe 66.5 %
66.5 %
Manganese, Mn 0.20 %
0.20 %
Molybdenum, Mo 5.25 %
5.25 %
Silicon, Si 0.40 %
0.40 %
Tungsten, W 10 %
10 %
Vanadium, V 3.1 %
3.1 %
Chemical Properties Metric English Comments
Critical Temperature 835 °C
1540 °F
Ac1