Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 840 °C | 1540 °F | Ac1 |
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications... |
|||
Critical Temperature | 840 °C | 1540 °F | Ac1 |
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13) TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu.. |
|||
Critical Temperature | 840 °C | 1540 °F | Ac1 |
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S) Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi.. |
|||
Critical Temperature | 840 °C | 1540 °F | Ac1 |
Latrobe DuraTechâ„¢ M4 High Carbon Powder Metal High Speed Steel (ASTM M4) DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v.. |
|||
Critical Temperature | 840 °C | 1540 °F | Ac1 |
Latrobe DuraTechâ„¢ M4 Powder Metal High Speed Steel (ASTM M4) DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v.. |