BASF Pluracol® 380 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 380 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 380 polyol is a high molecular weight, primary hydroxyl terminated triol. The combination of high molecular weight and reactivity makes Pluracol 380 useful in the preparation of elastomers and HR molded foams. Pluracol 380 has been formulated with a specialty inhibitor package which is not recommended for flexible slabstock foam production.Information provided by BASF
Physical Properties Metric English Comments
Density 0.989 g/cc

@Temperature 60.0 °C
0.0357 lb/in³

@Temperature 140 °F
1.01 g/cc

@Temperature 37.8 °C
0.0365 lb/in³

@Temperature 100 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 375 cP

@Temperature 60.0 °C
375 cP

@Temperature 140 °F
790 cP

@Temperature 37.8 °C
790 cP

@Temperature 100 °F
1370 cP

@Temperature 25.0 °C
1370 cP

@Temperature 77.0 °F
Molecular Weight 6500 g/mol
6500 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.010
<= 0.010
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color <30
APHA, STI 3057
Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 24 - 26 mg KOH/g
STI 3007/3162
Unsaturation <0.074 meq/g
STI 3056