BASF Pluracol® 2100 Slabstock HR Foam Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® 2100 Slabstock HR Foam Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Pluracol® 2100 polyol is a primary terminated conventional triol designed to be used in combination with Pluracol 2130 for the production of a broad range of slabstock HR foams. Pluracol 2100 polyol contains a LVI inhibitor package.Information provided by BASF
Physical Properties Metric English Comments
Density 0.989 g/cc

@Temperature 60.0 °C
0.0357 lb/in³

@Temperature 140 °F
1.01 g/cc

@Temperature 37.8 °C
0.0365 lb/in³

@Temperature 100 °F
1.02 g/cc

@Temperature 25.0 °C
0.0368 lb/in³

@Temperature 77.0 °F
Viscosity 375 cP

@Temperature 60.0 °C
375 cP

@Temperature 140 °F
790 cP

@Temperature 37.8 °C
790 cP

@Temperature 100 °F
1370 cP

@Temperature 25.0 °C
1370 cP

@Temperature 77.0 °F
Molecular Weight 6500 g/mol
6500 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.015
<= 0.015
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Clear Liquid
Hydroxyl Number 24 - 26 mg KOH/g
STI 3007/3162