Physical Properties Metric English Comments
Viscosity Test 62.0 - 112 cm³/g
62.0 - 112 cm³/g
Average value: 94.3 cm³/g Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Viscosity Test 62.0 - 111 cm³/g
62.0 - 111 cm³/g
Average value: 88.6 cm³/g Grade Count:31
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25..
Viscosity Test 62.0 - 86.0 cm³/g
62.0 - 86.0 cm³/g
Average value: 79.4 cm³/g Grade Count:12
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Copyright © lookpolymers.com All Rights Reserved