Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 62.0 - 112 cm³/g | 62.0 - 112 cm³/g | Average value: 94.3 cm³/g Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |