Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 62.0 - 86.0 cm³/g | 62.0 - 86.0 cm³/g | Average value: 79.4 cm³/g Grade Count:12 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |