Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 200 - 500 cP | 200 - 500 cP | RVF #3, 10 rpm, 424 |
PolyOne Aquamix™ 110 Latex Storage Stability: In excess of 6 months when stored under proper conditions in original sealed container. Keep from freezing. Water lost by evaporation can adversely affect viscosity, dispersabilit.. |
|||
Brookfield Viscosity | 250 - 500 cP | 250 - 500 cP | RVT (15% in MEK); MQSA 40 A |
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati.. |
|||
Brookfield Viscosity | 75 - 500 cP | 75 - 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 4125 Styrene-Butadiene Emulsion Applications: Rovene® 4125 is recommended for applications where a primer-sealer that provides adhesion between asphalt and other various surface treatments is needed. Rovene® 4125 has been us.. |
|||
Brookfield Viscosity | 100 - 500 cP | 100 - 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4150 SBR Latex ROVENE® 4150 is a medium-firm, self-XLing, carboxylated styrene-butadiene (SBR) latex emulsion. Its styrene content (55%) permits its use in formulating carpet and flooring mastics. This versatil.. |
|||
Brookfield Viscosity | 100 - 500 cP | 100 - 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 5051 Styrene-Butadiene Emulsion ROVENE® 5051 is a medium-firm, self cross-linking, carboxylated styrene-butadiene latex emulsion. Its styrene content permits the use in formulating carpet and flooring mastics. This versatile po.. |
|||
Brookfield Viscosity | 75 - 500 cP | 75 - 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6140 SBR Latex ROVENE® 6140 is a carboxylated styrene-butadiene emulsion that has a very soft and resilient hand that can be used for upholstery backcoating to produce fabrics showing high seam strengths. Due t.. |
|||
Brookfield Viscosity | 125 - 500 cP | 125 - 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Tite 445AF Skin packing / heat seal coating Description: Skin packing / heat seal coatingUsage: Michem® Tite 445AF is a coating which bonds heavily printed corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product i.. |
|||
Brookfield Viscosity | 250 - 500 cP | 250 - 500 cP | Spindle # 3, rpm 60 |
Michelman® SofTak® 317 Non-skid coating Description: Non-skid coating.Usage: SofTak® 317 is a gluable nonskid coating with excellent angle of skid. These properties are useful for slip or tier sheets, or a variety of other applications.. |
|||
Brookfield Viscosity | 250 - 500 cP @Temperature 25.0 °C |
250 - 500 cP @Temperature 77.0 °F |
10% Toluene solution |
Kraton® G1654 E (SEBS) Linear Block Copolymer Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass.Kraton G1654 ES - supplied as a "fluffy" crumb dusted wit.. |
|||
Brookfield Viscosity | 350 - 500 cP | 350 - 500 cP | RVT #3 @ 2.5 rpm |
3M Scotch-Weld™ HP69 Pipe Sealant Anaerobic Adhesives 3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. H.. |
|||
Brookfield Viscosity | 100 - 500 cP | 100 - 500 cP | Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/03 Linear Thermoplastic Polyurethane Pearlstick D40-70/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. Sol.. |
|||
Brookfield Viscosity | 150 - 500 cP | 150 - 500 cP | Spindle # 2, rpm 60 |
Michelman® StaticBan® 1005N Heat resistant conductive coating Heat resistant conductive coatingUsage: StaticBan® 1005N is a conductive coating which imparts a reliable, electrically conductive surface around sensitive electronic parts such as integrated circu.. |