Polymer Property : Brookfield Viscosity = 250 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 250 cP
250 cP
70% solids dispersed using a Brookfield #3 spindle at 100 rpm
Old Hickory M&M Clays, Inc. Wilco-SLU Kaolin Clay
Wilco SLU is an aqueous suspension of kaolin produced at 70% solids content. The slurry is deflocculated and rheology stabilized with sodium silicate. The Wilco SLU grade is a highly permeable selec..
Brookfield Viscosity 250 - 500 cP
250 - 500 cP
RVT (15% in MEK); MQSA 40 A
Lubrizol Advanced Materials PEARLBOND® 115 Linear Thermoplastic Polyurethane  (discontinued **)
PEARLBOND® 115 is a linear, aromatic polyurethane, supplied in form of white slightly yellowish pellets, which combines a very high crystallization rate with a high thermoplasticity level.Applicati..
Brookfield Viscosity 250 - 450 cP
250 - 450 cP
Spindle # 3, rpm 60
Michelman® Michem® Coat 40 Plus Water resistant, gluable coating
Description: Water resistant, gluable coatingUsage: Michem® Coat 40 Plus is a water-based coating designed to provide good water resistance to corrugated board while being cold set gluable with m..
Brookfield Viscosity 250 - 800 cP
250 - 800 cP
Spindle # 3, rpm 60
Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating
Description: Water resistant, cold set and hot melt gluable coatingUsage: Michem® Coat 40Y is a versatile water resistant coating. It is gluable with a wide range of water based and hot melt adhe..
Brookfield Viscosity 250 - 500 cP
250 - 500 cP
Spindle # 3, rpm 60
Michelman® SofTak® 317 Non-skid coating
Description: Non-skid coating.Usage: SofTak® 317 is a gluable nonskid coating with excellent angle of skid. These properties are useful for slip or tier sheets, or a variety of other applications..
Brookfield Viscosity 250 - 500 cP

@Temperature 25.0 °C
250 - 500 cP

@Temperature 77.0 °F
10% Toluene solution
Kraton® G1654 E (SEBS) Linear Block Copolymer
Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass.Kraton G1654 ES - supplied as a "fluffy" crumb dusted wit..
Brookfield Viscosity 250 cP
250 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane
Features: Soft compound with high elongation, displays low temperature flexibility and abrasion resistance. It can be processed by means of solution coating, extrusion and melt coating.Uses: Adhesiv..
Brookfield Viscosity 250 - 1000 cP
250 - 1000 cP
RVF #2 sp @ 20 rpm @ 80°F
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre..
Brookfield Viscosity 250 cP

@Temperature 25.0 °C
250 cP

@Temperature 77.0 °F
ASTM D2196-66; LVT
Lord Adhesives Aeroglaze® A276 Reflective Polyurethane
Aeroglaze® A276 reflective polyurethane gives a hard, flexible, colorfast, non-chalking surface that is resistant to most acids, alkaline detergents, lubricants, and chemicals.All information provi..