Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 350 cP @Temperature 25.0 °C |
350 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya COVERCARB® HP Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating. An opacifying product that is designed to reduce coating costs through the replacement of more expensive pigments. This product is .. |
|||
Brookfield Viscosity | 350 cP | 350 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 5588 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 5588 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Eu.. |
|||
Brookfield Viscosity | 350 - 650 cP | 350 - 650 cP | RVT (15% in MEK); MQSA 55 A |
Lubrizol Advanced Materials PEARLBOND® 108 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® 108 is a linear, aromatic polycaprolactone-based polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a medium thermoplasti.. |
|||
Brookfield Viscosity | 350 cP | 350 cP | |
Hybrid Plastics Fireban® Mark VI-IS Resorcinolinic (PRF) The resin system produces a superiour fire resistant material.Information provided by Hybrid Plastics |
|||
Brookfield Viscosity | 350 - 1200 cP | 350 - 1200 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4305 SBR Latex ROVENE® 4305 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This non-woven and textile binder offers outstanding.. |
|||
Brookfield Viscosity | 350 - 1200 cP | 350 - 1200 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 5005 SBR Latex ROVENE® 5005 is a carboxylated styrene-butadiene emulsion that has a very soft hand and neither contains nor evolves formaldehyde during cure. This paper saturant offers good water and solvent re.. |
|||
Brookfield Viscosity | <= 350 cP | <= 350 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Dispersion 275P Solvent dispersion of petroleum derived hydrocarbon Description: Solvent dispersion of petroleum derived hydrocarbonUsage: Michem® Dispersion 275P is designed to be used as a slip aid and scratch resistant additive in coil coatings.Information pro.. |
|||
Brookfield Viscosity | <= 350 cP | <= 350 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 70750 Cationic paraffin emulsion Description: Cationic paraffin emulsionUsage: Michem® Emulsion 70350 is designed to be a water repellent additive. This product is effectively used for the curing and protection of concrete.We se.. |
|||
Brookfield Viscosity | 350 - 2500 cP @Temperature 25.0 °C |
350 - 2500 cP @Temperature 77.0 °F |
25% solution in Toluene |
Sibur DST-30-01 2nd Group Styrene-Butadiene-Styrene Block Copolymer (SBS-TPE) Kraton D 1101, 1102. For modification of bitumen, intended for road coverings, modification of plastics, and for production of glues, strip hermetic, and protective coatings. |
|||
Brookfield Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 104 L Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 104 L: Same performa.. |
|||
Brookfield Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 108 A Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 108 A: Resin for van.. |
|||
Brookfield Viscosity | 350 - 450 cP @Temperature 25.0 °C |
350 - 450 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 902 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 902: Flexible resin .. |
|||
Brookfield Viscosity | 350 - 500 cP | 350 - 500 cP | RVT #3 @ 2.5 rpm |
3M Scotch-Weld™ HP69 Pipe Sealant Anaerobic Adhesives 3M™ Scotch-Weld™ Pipe Sealant Anaerobic Adhesives are one-component anaerobic sealants that cure and seal hydraulic and pneumatic pipes and fittings to withstand high temperatures and pressures. H.. |
|||
Brookfield Viscosity | 350 cP @Temperature 125 °C |
350 cP @Temperature 257 °F |
|
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Brookfield Viscosity | 350 cP | 350 cP | #1 spindle; 30 rpm |
DuPont Performance Polymers Neoprene 115 Polychloroprene
(discontinued **) Main feature: Mechanical stability methacrylic acid copolymer reactive. Principal uses include: Coatings, Modifiers, Asphalt, Concrete.Solids content: 47%. Initial pH: 7. Surface tension: 47 dyne.. |