Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 125 cP | 125 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highl.. |
|||
Brookfield Viscosity | 125 cP | 125 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 17-OR Anaerobic Thread Locking Compound BEARING AND SHAFT - SERIES 17-OR is a fast curing, GREEN, high strength, oil resistant, close fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highly .. |
|||
Brookfield Viscosity | <= 125 cP | <= 125 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 37135 Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 37135 provides mar and scratch resistance as well as some slip resistance when used as an additive in polishes and coatings.We s.. |
|||
Brookfield Viscosity | 125 cP | 125 cP | ASTM D2196, LVT, Spindle #2 @ 30rpm |
Lord Adhesives Chemglaze® V004 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Brookfield Viscosity | 125 - 500 cP | 125 - 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Tite 445AF Skin packing / heat seal coating Description: Skin packing / heat seal coatingUsage: Michem® Tite 445AF is a coating which bonds heavily printed corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product i.. |