Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 150 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
70% solids dispersed using a Brookfield #3 spindle at 100 rpm
Old Hickory M&M Clays, Inc. Wilco-LPC Kaolin Clay
Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SL..
Brookfield Viscosity 150 - 850 cP
150 - 850 cP
#20/200
Mallard Creek Polymers Rovene® 4119 Styrene-Butadiene Emulsion
Rovene® 4119 imparts a good wet/dry tensile strength, and has good adhesion to a wide variety of surfaces. As such, it makes an excellent base latex for paper and paperboard barrier coating appli..
Brookfield Viscosity 150 - 850 cP
150 - 850 cP
#20/200
Mallard Creek Polymers Tykote® 1019 Styrene-Butadiene Emulsion
Tykote® 1019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent film strength properties. It is intended for use as a base polymer in the formulation of barrier coat..
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
Spindle # 2, rpm 60
Michelman® DigiPrime® 5000 Primer
Description: Primer for digital printingUsage: DigiPrime® 5000 is a print primer which provides excellent adhesion of HP Indigo ElectroInks® to treated films and paper. It adheres well to many..
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
Spindle # 2, rpm 60
Michelman® DigiPrime® 5100 Primer
Description: Primer for digital printingUsage: DigiPrime® 5100 is a print primer which provides excellent adhesion of HP Indigo electro inks to treated films and paper. It adheres well to many sy..
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
Spindle # 3, rpm 60
Michelman® DigiPrime® 6029 Primer
Description: Primer for digital printingUsage: DigiPrime® 6029 is a flexo and gravure ready coating used to optimize substrates for HP Indigo printing. This product provides excellent adhesion of..
Brookfield Viscosity 150 - 650 cP
150 - 650 cP
Spindle # 3, rpm 60
Michelman® Michem® Coat 50 AFN Fluorocarbon free, water and grease resistant coating
Description: Fluorocarbon free, water and grease resistant coatingUsage: Michem® Coat 50AFN is an oil and grease resistant coating which also imparts good water resistance. This product is flexo ..
Brookfield Viscosity 150 - 400 cP

@Temperature 25.0 °C
150 - 400 cP

@Temperature 77.0 °F
LVT, Spindle #3 @ 30rpm
Lord Adhesives Flocklok® 853 Blocked Flock Adhesive
Flocklok® 853 is a blocked, heat-curing, single coat adhesive used to adhere polyester or nylon fibers (flock) to a variety of elastomers including EPDM, NR, CR, and SBR. Flocked substrates provi..
Brookfield Viscosity <= 150 cP
<= 150 cP
Spindle # 2, rpm 60
Michelman® Michem® Lube 368 Anionic paraffin/polyethylene wax emulsion
Description: Anionic paraffin/polyethylene wax emulsionUsage: Michem® Lube 368 is a water based emulsion which provides excellent water resistance and block resistance in paint and coating formul..
Brookfield Viscosity <= 150 cP
<= 150 cP
Spindle # 2, rpm 60
Michelman® Michem® Lube 743 Nonionic paraffin wax emulsion
Description: Nonionic paraffin wax emulsionUsage: Michem® Lube 743 exhibits a high degree of water resistance and excellent compatibility. This product is used in many water based coating applica..
Brookfield Viscosity 150 - 400 cP
150 - 400 cP
Spindle # 3, rpm 60
Michelman® VaporBase™ 1065 MVTR primer
Description: MVTR primerUsage: VaporBase™ 1065 is a primer designed to be used in tandem with the VaporCoat® series of products. VaporBase™ 1065 works to seal the base substrate allowin..
Brookfield Viscosity 150 - 400 cP
150 - 400 cP
Spindle # 3, rpm 60
Michelman® VaporBase™ 1075 Water resistance primer
Description: Water resistance primerUsage: VaporBase™ 1075 is a primer designed to be used in tandem with the VaporCoat® series of products as well as others. VaporBase™ 1075 works to s..
Brookfield Viscosity <= 150 cP
<= 150 cP
SIR-3 (JIS Z8802)
Kraton® Cariflex™ IR0401 SU Polyisoprene Rubber Latex
Description: Cariflex IR0401 SU Latex is a water-based emulsion of an anionically polymerized polyisoprene with a high cis-1,4 content, high molecular weight and a high linearity. The emulsion also..
Brookfield Viscosity 150 - 850 cP
150 - 850 cP
Spindle # 3, rpm 60
Michelman® Michem® Tite 335AF Skin packing / heat seal coating
Description: Skin packing / heat seal coatingUsage: Michem® Tite 335AF is a coating which bonds corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product in between. Adhes..
Brookfield Viscosity 150 - 450 cP
150 - 450 cP
Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 45-90/03 Polycaprolactone based TPU
Pearlstick 45-90/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization..
Brookfield Viscosity 150 cP

@Temperature 125 °C
150 cP

@Temperature 257 °F
Westlake Epolene® N-14 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-14 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Brookfield Viscosity 150 cP

@Temperature 125 °C
150 cP

@Temperature 257 °F
Westlake Epolene® N-14P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Description: Epolene N-14P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..
Brookfield Viscosity 150 cP

@Temperature 25.0 °C
150 cP

@Temperature 77.0 °F
Loctite® 3301 Light Cure Acrylic Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Brookfield Viscosity 150 cP

@Temperature 200 °C
150 cP

@Temperature 392 °F
Melt
Zeon Chemicals Quintone® D100 Aliphatic Hydrocarbon Resin
C5/C9 type (piperylene and dicyclopentadiene precursor). Has improved compatibility with SBR and EVA; suitable for adhesive tapes and hot-melt adhesives.Information provided by Zeon Chemicals L.P.
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
#2 @ 50 rpm
Dow Latex XZ 92226.00 Experimental Latex
Description: XZ 92226.00 Experimental latex is an aqueous dispersion of a modified carboxylated styrene butadiene copolymer. It has been developed for use as latex for precoating and adhesive for se..
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
3M 32661 Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
3M 32662 Black Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
3M 32665 Green Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
3M 32666 Tan Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Brookfield Viscosity 150 - 500 cP
150 - 500 cP
Spindle # 2, rpm 60
Michelman® StaticBan® 1005N Heat resistant conductive coating
Heat resistant conductive coatingUsage: StaticBan® 1005N is a conductive coating which imparts a reliable, electrically conductive surface around sensitive electronic parts such as integrated circu..
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
3M 32663 Medium Grey Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Brookfield Viscosity 150 - 1250 cP
150 - 1250 cP
RVT Model, Spindle #3 @ 20 rpm
3M 32664 Light Gray Heavy Duty Performance Coating - Part B
3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and ..
Brookfield Viscosity 150 cP

@Temperature 25.0 °C
150 cP

@Temperature 77.0 °F
Extrusion rate, grams/minute, 1/8" orifice at 90 psi
Loctite® Nuva-Sil® 5084 Sealant
Silicon Light Cure Adhesives and Gasketing and Wire TackersLoctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazard..
Brookfield Viscosity <= 150 cP
<= 150 cP
KM 44
Kraton® Cariflex™ IR0401 BU Polyisoprene Rubber Latex
Description: Cariflex™ IR0401 BU Latex is a water-based emulsion of an anionically polymerized polyisoprene with a high cis-1,4 content, high molecular weight and a high linearity. The emulsion al..
Copyright © lookpolymers.com All Rights Reserved