Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 405 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 405 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Goo.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 406 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 406 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Goo.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 440 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 440 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Eur.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 455 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 455 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Goo.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® CC 136 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® CC 136 is an aqueous dispersion of a modified carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers.Key Features: Europrene Latice® CC 136 shows .. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya COVERCARB® 85 Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating that is designed to provide maximum opacity and maximum gloss. It is an excellent choice to reduce the demand for expensive pigments.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
No. 3 Spindle, 100 rpm |
Omya HYDROCARB® HG Calcium Carbonate An ultrafine ground calcium carbonate for paper and board coating.Information supplied by Omya North America. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 171 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 4195 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 171 is an ultra-high molecular weight, fine particle size homopolymer dispersion resin intended for use in thin, organosol cast coatings and films. This resin provides excellent fused film an.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Day Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Day Viscosity @ 30 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Hour Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L140UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L140UF is an ultra high molecular weight, ultrafine particle size homopolymer dispersion resin. The excellent dispersibility provides good product throughput during the organoso.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | 20 rpm; ASTM D1417 |
Polimeri Europa Europrene Latice® 5583 Carboxylated Styrene - Butadiene Copolymer Europrene Latice® 5583 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers. It contains a non staining antioxidant.Key Features: Go.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | One Day Viscosity @ 30rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 174 is a medium molecular weight, fine particle size homopolymer dispersion resin. It provides a good balance of fused film properties and processing temperatures. It is recommended for appli.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | #20/200 |
Mallard Creek Polymers Rovene® 6018 Styrene-Acrylic Emulsion Applications: Rovene® 6018 is a silanated styrene-acrylic emulsion specifically designed for formulation of construction adhesives such as ceramic tile mastics and carpet adhesives. It provides e.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | #20/200 |
Mallard Creek Polymers Rovene® 6118 Styrene-Acrylic Emulsion Applications: Rovene® 6118 is a silanated styrene-acrylic emulsion specifically designed for formulation of concrete sealers and performance coatings. It provides excellent adhesion to concrete a.. |
|||
Brookfield Viscosity | 300 - 700 cP | 300 - 700 cP | Spindle # 3, rpm 60 |
Michelman® Coating X300™ Plus Water based, moisture and water resistant coating Description: Water based, moisture and water resistant coating.Usage: Coating X300™ Plus provides high levels of water resistance and good moisture resistance for kraft paper with improved wate.. |
|||
Brookfield Viscosity | 300 - 750 cP | 300 - 750 cP | Spindle # 3, rpm 20 |
Michelman® Michem® Coat 95 Water and grease resistant, heat sealable coating Description: Water and grease resistant, heat sealable coatingUsage: Michem® Coat 95 is a good multi-purpose coating that provides excellent water, oil and grease resistance. This product is heat.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
ASTM D2196-86; LVT |
Lord Adhesives Aeroglaze® Z307 Absorptive Conductive Polyurethane Aeroglaze® Z307 black absorptive conductive polyurethane coating is primarily for application to substrates used on spacecraft. These applications include those where coatings must exhibit low ou.. |
|||
Brookfield Viscosity | <= 300 cP | <= 300 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 91240G Nonionic polyethylene emulsion Description: Nonionic polyethylene emulsionUsage: Michem® Emulsion 91240G is an additive which provides excellent anti-blocking, slip properties and mar resistance. It is also used as an additive.. |
|||
Brookfield Viscosity | 300 - 800 cP | 300 - 800 cP | Spindle # 3, rpm 60 |
Michelman® Release Coat® P1 Uncatalyzed portion of a two-part silicone release coating Description: Uncatalyzed portion of a two-part silicone release coatingUsage: Release Coat® P1 is one part of a two part silicone release coating. A catalyzed release coat system offers superior .. |
|||
Brookfield Viscosity | 300 cP @Temperature 190 °C |
300 cP @Temperature 374 °F |
|
Westlake Epolene® E-43 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-43 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Brookfield Viscosity | 300 cP @Temperature 190 °C |
300 cP @Temperature 374 °F |
|
Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer Description: Epolene E-43P is a maleic anhydride grafted polypropylene powder recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Brookfield Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
|
Loctite® 363 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 300 cP | 300 cP | #2 @ 50 rpm |
Dow HPL 502 Carboxylated Terpolymer Latex Applications: HPL*502 Latex is part of Dow’s HPL* Latex family of the high-performance ignition resistant latexes. HPL* latexes offer properties not available in standard styrene-butadiene latexes... |
|||
Brookfield Viscosity | 300 cP | 300 cP | / 3 rpm; spindle #2 |
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating AboCoat 8204-15 is a flammable light-blue liquid resin. AboCure 8204-115 is a flammable clear amber liquid converter. AboCoat 8204-15/AboCure 8204-15 is a dielectric coating for high chemical, solve.. |
|||
Brookfield Viscosity | 300 - 400 cP @Temperature 25.0 °C |
300 - 400 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 103 L Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 103 L: Light-stabili.. |
|||
Brookfield Viscosity | 300 - 1000 cP | 300 - 1000 cP | LFT, #3 sp @ 2.5 rpm |
3M Scotch-Weld™ RT300B Rubber-Toughened Instant Adhesive 3M™ Scotch-Weld™ Rubber Toughened Instant Adhesives are formulated with a unique elastomer that maximizes impact, vibration, peel, and thermal cycling resistance while providing tough flexible bon.. |
|||
Brookfield Viscosity | 300 - 1300 cP | 300 - 1300 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4457 SBR Latex ROVENE® 4457 is a highly carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is crosslinkable with extern.. |