Polymer Property : Brookfield Viscosity = 800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 400 - 800 cP

@Temperature 20.0 °C
400 - 800 cP

@Temperature 68.0 °F
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A
Lubrizol Advanced Materials Pearlstick® 45-50/05 Linear Thermoplastic Polyurethane Elastomer  (discontinued **
Pearlstick 45-50/05 is an elastic, linear, aromatic polyurethane with an extremely high crystallization rate and a medium-low thermoplasticity level, available as pellets.Solubility: Pearlstick 45-..
Brookfield Viscosity 200 - 800 cP
200 - 800 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4220 SBR Emulsion
ROVENE® 4220 is a new developmental polymer specifically designed to be used flooring adhesives as well as an extender for chloroprene and natural latex in contact adhesives and other cohesive an..
Brookfield Viscosity 175 - 800 cP
175 - 800 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4310 SBR Latex
ROVENE® 4310 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip” applications. This non-woven, textile, and p..
Brookfield Viscosity 300 - 800 cP
300 - 800 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4402 SBR Latex
ROVENE® 4402 is a carboxylated styrene-butadiene emulsion which does not contain nor evolve formaldehyde during cure. ROVENE® 4402 has a medium soft hand with outstanding strength properties. ..
Brookfield Viscosity 200 - 800 cP
200 - 800 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 4848 SBR Emulsion
ROVENE® 4848 is a new developmental polymer specifically designed to be used in two part spray adhesives for open or closed cell foams and other contact and cold seal applications. Fast breaking ..
Brookfield Viscosity 175 - 800 cP
175 - 800 cP
#2/20 rpm
Mallard Creek Polymers ROVENE® 5010 SBR Latex
ROVENE® 5010 is a carboxylated styrene-butadiene emulsion that imparts an ultra soft hand when used in backcoating, spray, and “dip and nip” applications. This non-woven, textile, and p..
Brookfield Viscosity 400 - 800 cP
400 - 800 cP
Spindle # 3, rpm 60
Michelman® HydroGrease White™ 22 White coating
Description: High performance water and grease resistant white coatingUsage: HydroGrease Whiteâ„¢ 22 is a white coating which imparts water and grease resistance to the substrate. This coating is..
Brookfield Viscosity 250 - 800 cP
250 - 800 cP
Spindle # 3, rpm 60
Michelman® Michem® Coat 40Y Water resistant, cold set and hot melt gluable coating
Description: Water resistant, cold set and hot melt gluable coatingUsage: Michem® Coat 40Y is a versatile water resistant coating. It is gluable with a wide range of water based and hot melt adhe..
Brookfield Viscosity 300 - 800 cP
300 - 800 cP
Spindle # 3, rpm 60
Michelman® Release Coat® P1 Uncatalyzed portion of a two-part silicone release coating
Description: Uncatalyzed portion of a two-part silicone release coatingUsage: Release Coat® P1 is one part of a two part silicone release coating. A catalyzed release coat system offers superior ..
Brookfield Viscosity 600 - 800 cP

@Temperature 25.0 °C
600 - 800 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 401 Isophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 401: Food-grade resi..
Brookfield Viscosity 600 - 800 cP

@Temperature 25.0 °C
600 - 800 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 402 Isophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 402: High-quality re..
Brookfield Viscosity 400 - 800 cP
400 - 800 cP
RVT #2 spindle @ 20 rpm
3M Scotch-Weld™ RT40 Retaining Compound Anaerobic Adhesives
3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings..