Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® E-43P Oxidized Low Molecular Weight Polyethylene Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Epolene E-43P is a maleic anhydride grafted polypropylene powder recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emulsions. Because of the polarity and anhydride functionality, Epolene E-43P is useful for laminating, as a compatibilizer for PP blends with nylon or EVOH, and for enhancing the strength of composites that utilize reinforcements / fillers such as glass, talc, calcium carbonate, and metals. Key Attributes:Coupling agent and compatibilizer for PP composites and alloysExcellent pigment dispersion aidMaleic anhydride grafted polypropylene (PP)Provides slip resistance in floor polish finishesUseful in adhesive blends Application/Uses:AutomotiveBookbindingBuilding and ConstructionCaulks and SealantsHot Melt AdhesivesLaminatingSolventborne AdhesivesWaterborne Adhesives Information provided by Westlake Chemical
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D5
Viscosity 100 - 750 cP

@Temperature 190 °C
100 - 750 cP

@Temperature 374 °F
542-111
Brookfield Viscosity 300 cP

@Temperature 190 °C
300 cP

@Temperature 374 °F
Molecular Weight 9100 g/mol
9100 g/mol
Thermal Properties Metric English Comments
Flash Point >= 277 °C
>= 531 °F
Ring & Ball Softening Point 158 °C
316 °F
Optical Properties Metric English Comments
Gardner Color Number <= 13
<= 13
542-130
Chemical Properties Metric English Comments
Total Acid Number 45
45
mg KOH/g
Descriptive Properties Value Comments
Penetration Hardness <1 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 °C