Dow HPL 502 Carboxylated Terpolymer Latex

Category Polymer
Manufacturer Dow Chemical
Trade Name HPL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow HPL 502 Carboxylated Terpolymer Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: HPL*502 Latex is part of Dow’s HPL* Latex family of the high-performance ignition resistant latexes. HPL* latexes offer properties not available in standard styrene-butadiene latexes. HPL* latex products have chlorine content reacted into the backbone of the polymer that provides a “built in” level of ignition resistance. This inherent ignition resistance enables the formulator to displace some or all of the alumina trihydrate (ATH) with less costly calcium carbonate filler which may result in substantial compound cost savings. The presence of chlorine in the polymer backbone also allows the use of an antimony synergist without the addition of expensive additives. HPL* latexes are used in the precoat compound for both commercial and residential carpet backing applications. HPL* latexes are also used in unitary and tile backing applications.Benefits: High SolidsIgnition ResistantBlister ResistantMedium HandInformation provided by Styron
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
Solids Content 57 %
57 %
Particle Size 1.25 µm
1.25 µm
pH 7.0
7.0
Brookfield Viscosity 300 cP
300 cP
#2 @ 50 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 9.50 °C
49.1 °F
Oxygen Index 26 %
26 %
0 ATH Load
30 %
30 %
200 ATH Load
36 %
36 %
400 ATH Load
40 %
40 %
600 ATH Load
Descriptive Properties Value Comments
Minimum film formation temperature 48.2°F