3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neoprene, reclaim, SBR, and butyl rubber. They have high immediate strength and excellent heat resistance. 3M Scotch-Weld Adhesive 1300L is a lower solids, lower viscosity version of 3M Scotch-Weld Adhesive 1300.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 26 - 33 %
26 - 33 %
Brookfield Viscosity 250 - 1000 cP
250 - 1000 cP
RVF #2 sp @ 20 rpm @ 80°F
Mechanical Properties Metric English Comments
Shear Strength 0.586 MPa
85.0 psi
0.586 MPa

@Temperature 107 °C,
Time 1.81e+6 sec
85.0 psi

@Temperature 225 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
0.938 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
136 psi

@Temperature 180 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
1.34 MPa

@Temperature -34.0 °C,
Time 1.81e+6 sec
195 psi

@Temperature -29.2 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
2.36 MPa

@Temperature 75.0 °C,
Time 1.21e+6 sec
343 psi

@Temperature 167 °F,
Time 336 hour
Overlap, 1/8" Birch/Birch
3.79 MPa

@Temperature 75.0 °C,
Time 1.81e+6 sec
549 psi

@Temperature 167 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
Peel Strength 3.16 kN/m

@Temperature 24.0 °C,
Time 86400 sec
18.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
4.56 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
26.0 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
5.26 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
30.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
5.70 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
32.5 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
8.41 kN/m

@Temperature 24.0 °C,
Time 259000 sec
48.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
8.59 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
49.0 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
8.94 kN/m

@Temperature 24.0 °C,
Time 432000 sec
51.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
9.12 kN/m

@Temperature 24.0 °C,
Time 605000 sec
52.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -26.0 °C
-14.8 °F
TCC
Descriptive Properties Value Comments
Appearance Yellow
Base Polychloroprene