Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brookfield Viscosity = 450 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 250 - 450 cP
250 - 450 cP
Spindle # 3, rpm 60
Michelman® Michem® Coat 40 Plus Water resistant, gluable coating
Description: Water resistant, gluable coatingUsage: Michem® Coat 40 Plus is a water-based coating designed to provide good water resistance to corrugated board while being cold set gluable with m..
Brookfield Viscosity 180 - 450 cP

@Temperature 23.0 °C
180 - 450 cP

@Temperature 73.4 °F
Lucite International Series 100 Liquid Acrylic Resin
LUCITE® LIQUID ACRYLIC RESINS SERIES 100For the manufacture of solid surface shapesAmbient temperature cureCan be used on batch or continuous in-line mixing equipmentInformation provided by Lucit..
Brookfield Viscosity 150 - 450 cP
150 - 450 cP
Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 45-90/03 Polycaprolactone based TPU
Pearlstick 45-90/03 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization..
Brookfield Viscosity 350 - 450 cP

@Temperature 25.0 °C
350 - 450 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 104 L Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 104 L: Same performa..
Brookfield Viscosity 350 - 450 cP

@Temperature 25.0 °C
350 - 450 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 108 A Orthophthalic Resin
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 108 A: Resin for van..
Brookfield Viscosity 350 - 450 cP

@Temperature 25.0 °C
350 - 450 cP

@Temperature 77.0 °F
C.O.I.M. EXTER S® S 902 Special Laminate
Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 902: Flexible resin ..
Brookfield Viscosity 200 - 450 cP
200 - 450 cP
RVF #2 sp @ 20 rpm @ 80°F
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat..
Copyright © lookpolymers.com All Rights Reserved