Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | DOP 60phr, 6RPM; ASTM D1824-90 |
LG Chemical LP170L PVC General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for .. |
|||
Brookfield Viscosity | 2000 - 6000 cP | 2000 - 6000 cP | DOP 60phr; ASTM D1824 |
LG Chemical PB1202 PVC General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin.. |
|||
Brookfield Viscosity | 2000 - 3000 cP | 2000 - 3000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 48440 Polymer solution Description: Polymer solutionUsage: Michem® Emulsion 48440 is used for fiber sizing.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint .. |
|||
Brookfield Viscosity | 2000 cP @Temperature 25.0 °C |
2000 cP @Temperature 77.0 °F |
|
Loctite® 3761 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 2000 cP | 2000 cP | 0.1; MA 04-3-064 |
Dynasol Calprene® H6171 Hydrogenated Rubber (SEBS) Calprene H6171 is a 67/33 ethylene-butylene/styrene thermoplastic copolymer, polymerized in solution and having a high molecular weight, a linear structure and with excellent ozone resistance. Appli.. |
|||
Brookfield Viscosity | 2000 cP @Temperature 23.9 °C |
2000 cP @Temperature 75.0 °F |
|
BCC Products BC 5105 Epoxy Laminating System BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. .. |
|||
Brookfield Viscosity | 2000 cP | 2000 cP | A Component; Spindle #3; speed 10 rpm; ASTM D1824 |
Aptek 6103-A/B Epoxy Encapsulant Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided.. |
|||
Brookfield Viscosity | 2000 - 4000 cP | 2000 - 4000 cP | RVF #3 sp @ 10 rpm |
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a.. |
|||
Brookfield Viscosity | 2000 - 8000 cP | 2000 - 8000 cP | Base, RVF #7 spindle, 20 rpm @ 27°C |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |
|||
Brookfield Viscosity | 2000 - 8000 cP | 2000 - 8000 cP | Base, RFV #7 at 20 rpm |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Brookfield Viscosity | 2000 - 2400 cP | 2000 - 2400 cP | Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-50/22 Polycaprolactone based TPU Pearlstick 45-50/22 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium-low thermoplasticity levelSolu.. |