Material Notes:
General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for synthetic leather foam layer made by Knife coating/ Roll coating/ Gravure coating especially, products made from LP170L are excellent in restoring force and print ability.Main Applications: Slush molding, synthetic leather, gloveCAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.406 g/cc
1.406 g/cc
Bulk Density 0.290 - 0.390 g/cc
0.0105 - 0.0141 lb/in³
ASTM D1895
Volatiles <= 1.5 %

@Temperature 110 °C,
Time 3600 sec
<= 1.5 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Brookfield Viscosity 2000 - 4000 cP
2000 - 4000 cP
DOP 60phr, 6RPM; ASTM D1824-90
Viscosity Measurement >= 1.0

@Pressure 0.400 MPa
>= 1.0

@Pressure 58.0 psi
[g/sec], DOP 60phr, Severs; ASTM D1823-90
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 1600-1700
30°C, JIS K6721-77
K-Value 76
DIN53726