Brookfield Viscosity 2000 - 4000 cP
2000 - 4000 cP
DOP 60phr, 6RPM; ASTM D1824-90
LG Chemical LP170L PVC
General Description: LP170L, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170L can be used for ..
Brookfield Viscosity 2000 - 6000 cP
2000 - 6000 cP
DOP 60phr; ASTM D1824
LG Chemical PB1202 PVC
General Description: PB1202, homopolymer made by micro-suspension seeded polymerization, PVC Resin has a fluid property similar to Newtonian fluidity (low-viscosity) It is mainly used for non-foamin..
Brookfield Viscosity 2000 - 3000 cP
2000 - 3000 cP
Spindle # 3, rpm 60
Michelman® Michem® Emulsion 48440 Polymer solution
Description: Polymer solutionUsage: Michem® Emulsion 48440 is used for fiber sizing.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint ..
Brookfield Viscosity 2000 cP

@Temperature 25.0 °C
2000 cP

@Temperature 77.0 °F
Loctite® 3761 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Brookfield Viscosity 2000 cP
2000 cP
0.1; MA 04-3-064
Dynasol Calprene® H6171 Hydrogenated Rubber (SEBS)
Calprene H6171 is a 67/33 ethylene-butylene/styrene thermoplastic copolymer, polymerized in solution and having a high molecular weight, a linear structure and with excellent ozone resistance. Appli..
Brookfield Viscosity 2000 cP

@Temperature 23.9 °C
2000 cP

@Temperature 75.0 °F
BCC Products BC 5105 Epoxy Laminating System
BC 5105 is a clear, unfilled, low viscosity laminating system. This heat resistant resin exhibits excellent wet out, reasonable working time and may be used at room temperature without post-curing. ..
Brookfield Viscosity 2000 cP
2000 cP
A Component; Spindle #3; speed 10 rpm; ASTM D1824
Aptek 6103-A/B Epoxy Encapsulant
Optoelectronic grade, reddish black encapsulant for IR LED discreets. Transparent to IR light while blocking out visible light.Part A is deep red. Part B is clear to pale yellow.Information provided..
Brookfield Viscosity 2000 - 4000 cP
2000 - 4000 cP
RVF #3 sp @ 10 rpm
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a..
Brookfield Viscosity 2000 - 8000 cP
2000 - 8000 cP
Base, RVF #7 spindle, 20 rpm @ 27°C
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..
Brookfield Viscosity 2000 - 8000 cP
2000 - 8000 cP
Base, RFV #7 at 20 rpm
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M
Brookfield Viscosity 2000 - 2400 cP
2000 - 2400 cP
Brookfield RVF sp 5, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A
Lubrizol Advanced Materials Pearlstick® 45-50/22 Polycaprolactone based TPU
Pearlstick 45-50/22 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium-low thermoplasticity levelSolu..