Material Notes:
Wilco LPC is the same selection as the SLU grade except it is in natural shredded or Airfloat (powdered) form. It offers the same benefits in a ceramic casting formulation discussed above for the SLU product.Information provided by Old Hickory Clay Company
Physical Properties Metric English Comments
Specific Gravity 2.62 g/cc
2.62 g/cc
Bulk Density 3.59 g/cc
0.130 lb/in³
Moisture Absorption <= 1.00 %
<= 1.00 %
Particle Size 0.50 µm
0.50 µm
21.8% of partciles less than
1.0 µm
1.0 µm
36.8% of particles less than
2.0 µm
2.0 µm
Median particle diameter
2.0 µm
2.0 µm
50.0% of particles less than
5.0 µm
5.0 µm
72.3% of particles less than
10 µm
10 µm
87.7% of particles less than
<= 20 µm
<= 20 µm
95.9% of particles less than
pH 4.5 - 6.5
4.5 - 6.5
10% solids
Specific Surface Area 10 m²/g
10 m²/g
Brookfield Viscosity 150 - 300 cP
150 - 300 cP
70% solids dispersed using a Brookfield #3 spindle at 100 rpm
Component Elements Properties Metric English Comments
Al2O3 38.21 %
38.21 %
CaO 0.040 %
0.040 %
Fe2O3 0.36 %
0.36 %
K2O 0.11 %
0.11 %
Loss on Ignition(%) 13.51 %
13.51 %
MgO 0.020 %
0.020 %
Na2O 0.020 %
0.020 %
SiO2 45.16 %
45.16 %
TiO2 1.77 %
1.77 %
Descriptive Properties Value Comments
Casting Rate (Barold) 120
CEC/MBI (meg/100 ml) 2
Pyrometric Cone Equivalent (PCE) 34
Wet Sieve Residue (%) 1
Wet Sieve Residue, +325 mesh