Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.0100 cc-mm/m²-24hr-atm | 0.0254 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® DC3203F Ethylene Vinyl Alcohol Copolymer Low ethylene content. Suitable for use in packaging material used at normal temperature and humidity. Ethylene content 32 mol%. Volatile matter 0.3%.Information provided by Soarus, LLC. In the Un.. |
|||
Oxygen Transmission | 0.0100 cc-mm/m²-24hr-atm | 0.0254 cc-mil/100 in²-24hr-atm | 20°C- 65% RH; based on 20 µm layer |
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Oxygen Transmission | 0.0100 cc-mm/m²-24hr-atm | 0.0254 cc-mil/100 in²-24hr-atm | 23°C- 55% RH; Film; based on 20 µm layer |
Noltex Soarnol® MS3203 Ethylene Vinyl Alcohol Copolymer Modified DC3203; New improved thermoformable EVOH. Ethylene content 32 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon .. |
|||
Oxygen Transmission | 0.0100 cc-mm/m²-24hr-atm | 0.0254 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |