Material Notes:
Low ethylene content. Suitable for use in packaging material used at normal temperature and humidity. Ethylene content 32 mol%. Volatile matter 0.3%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Moisture Vapor Transmission 1.14 cc-mm/m²-24hr-atm
2.90 cc-mil/100 in²-24hr-atm
based on 30 µm layer
Oxygen Transmission 0.0100 cc-mm/m²-24hr-atm
0.0254 cc-mil/100 in²-24hr-atm
20°C- 65% RH; based on 20 µm layer
Viscosity 1.40e+7 cP

@Shear Rate 120 1/s,
Temperature 230 °C
1.40e+7 cP

@Shear Rate 120 1/s,
Temperature 446 °F
Melt Flow 3.2 g/10 min

@Load 2.16 kg,
Temperature 210 °C
3.2 g/10 min

@Load 4.76 lb,
Temperature 410 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
DSC, both heating and cooling speeds of 10°C/min
Crystallization Temperature 158 °C
316 °F
DSC, both heating and cooling speeds of 10°C/min
Glass Transition Temp, Tg 63.0 °C
145 °F
DSC, both heating and cooling speeds of 10°C/min
Optical Properties Metric English Comments
Refractive Index 1.524
1.524
Quenched
1.533
1.533
Annealed at 140°C, 30 min
Haze 0.50 %
0.50 %
Processing Properties Metric English Comments
Nozzle Temperature 200 - 220 °C
392 - 428 °F