Noltex Soarnol® MS3203 Ethylene Vinyl Alcohol Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Alcohol (EVOH)
Manufacturer Noltex
Trade Name Soarnol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Noltex Soarnol® MS3203 Ethylene Vinyl Alcohol Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified DC3203; New improved thermoformable EVOH. Ethylene content 32 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippon Gohsei.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Oxygen Transmission 0.0100 cc-mm/m²-24hr-atm
0.0254 cc-mil/100 in²-24hr-atm
23°C- 55% RH; Film; based on 20 µm layer
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 210 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 410 °F
Thermal Properties Metric English Comments
Melting Point 181 °C
358 °F
Crystallization Temperature 160 °C
320 °F
Optical Properties Metric English Comments
Refractive Index 1.524
1.524
Quenched
1.533
1.533
Annealed at 140°C, 30 min