Physical Properties Metric English Comments
Melt Flow 42 g/10 min

@Load 10.0 kg,
Temperature 220 °C
42 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
SABIC Innovative Plastics Cycolac® MG94 ABS
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
Melt Flow 42 g/10 min

@Load 5.00 kg,
Temperature 200 °C
42 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro..
Melt Flow 42 g/10 min

@Load 1.20 kg,
Temperature 300 °C
42 g/10 min

@Load 2.65 lb,
Temperature 572 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
SABIC Innovative Plastics Lexan® OQ1060 PC Copolymer
Optical quality, high flow, high purity Polycarbonate copolymer resin with reduced oxygen transmission for advanced DVD applications such as Limited Play DVD.This data was supplied by SABIC-IP for t..
Melt Flow 42 - 56 g/10 min

@Load 21.6 kg,
Temperature 190 °C
42 - 56 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283
NIZHNEKAMSKNEFTEKHIM PE 6753G (526H7) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Melt Flow 42 - 94.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
42 - 94.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene
Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez
Melt Flow 42 g/10 min

@Load 5.00 kg,
Temperature 300 °C
42 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Noryl V01505 PPE+HIPS
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Flow 42 g/10 min

@Load 5.00 kg,
Temperature 300 °C
42 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Noryl V01505 PPE+HIPS (Asia Pacific)
Noryl* V01505 is a 15% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Flow 42 g/10 min

@Load 5.00 kg,
Temperature 300 °C
42 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific)
Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade.
Melt Flow 42 g/10 min

@Load 5.00 kg,
Temperature 280 °C
42 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
SABIC Innovative Plastics Noryl PX0003 PPE+HIPS
PX0003 resin is a modified PPE+PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gr..
Melt Flow 42 g/10 min

@Load 10.0 kg,
Temperature 220 °C
42 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO-1133
Chi Mei Polylac® PA-765B ABS - Flame Retardant
F.R. Medium Impact
Melt Flow 42 g/10 min

@Load 3.80 kg,
Temperature 200 °C
42 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Melt Flow 42 g/10 min

@Load 3.80 kg,
Temperature 200 °C
42 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Europe-Africa-Middle East)
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Melt Flow 42 g/10 min

@Load 3.80 kg,
Temperature 200 °C
42 g/10 min

@Load 8.38 lb,
Temperature 392 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2060 PPE+PS
Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR ..
Copyright © lookpolymers.com All Rights Reserved