Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42 - 94.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
42 - 94.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT 18-11 Linear Low Density Polyethylene Production Method: Gaseous-phase method. Application: Composition is intended to be processed into a stretch film.Information Provided by Kazanorgsintez |