Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Europe-Africa-Middle East) Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Melt Flow | 13 g/10 min @Load 3.80 kg, Temperature 230 °C |
13 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 210 °C |
13 g/10 min @Load 4.76 lb, Temperature 410 °F |
ASTM D1238 |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 220 °C |
13 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Melt Flow | 13 g/10 min @Load 6.60 kg, Temperature 337 °C |
13 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2412EPR PEI 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 266 °C |
13 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® PL 10 HDPE Pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VL 10 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Xmod™ MC55 High Crystalline Polypropylene Copolymer Xmod MC55 is a HCPP intended for injection molding of automotive interior parts. Xmod MC55 has an excellent balance between impact strength and stiffness as well as good surface quality.Xmod MC55 h.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 240 °C |
13 g/10 min @Load 4.76 lb, Temperature 464 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Melt Flow | 13 g/10 min @Load 3.80 kg, Temperature 230 °C |
13 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA TWP 121 Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 275 °C |
13 g/10 min @Load 22.0 lb, Temperature 527 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PA 1408 Conductive Thermoplastic Compound PRE-ELEC® PA 1408 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1.. |