Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX3415 PC Copolymer Lexan* DMX3415 is a co-polycarbonate resin with improved scratch resistance, high purity and optical quality.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTPM309 ASA+PC (Europe-Africa-Middle East) XTPM309 is a modified HRA170 with improved processing stability.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 13 g/10 min @Load 21.6 kg, Temperature 190 °C |
13 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) MF3713 High Density Polyethylene MF3713 is a high molecular weight high density polyethylene.Applications: bags, products for use in property modification.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 220 °C |
13 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 220 °C |
13 g/10 min @Load 11.0 lb, Temperature 428 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1000V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in .. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 340 °C |
13 g/10 min @Load 11.0 lb, Temperature 644 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 1010RF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg.. |
|||
Melt Flow | 13 g/10 min @Load 6.60 kg, Temperature 337 °C |
13 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East) 40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® IQ1103R PBT+PC Xenoy* Resin iQ1103R - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103R is an unreinforced, impact modified PC + iQ-PBT alloy with excellent low temperature im.. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM Test |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 265 °C |
13 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® XD549S PBT+PC (Europe-Africa-Middle East) Xenoy XD549S is an automotive grade, designed for thin wall (2.5 mm.) direct gated exterior parts. The material has an excellent flow. Xenoy XD549S can be painted with primerless solvent or waterbas.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 300 °C |
13 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |
|||
Melt Flow | 13 g/10 min @Load 10.0 kg, Temperature 220 °C |
13 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-747 ABS High impact |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very .. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Melt Flow | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Melt Flow | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
Melt Flow | 13 g/10 min @Load 3.80 kg, Temperature 200 °C |
13 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East) VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry. |