Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylac® FR134 ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylac® FR134 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ravago.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 5.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
13 g/10 min

@Load 3.80 kg,
Temperature 230 °C
13 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Yield Strength 60.7 MPa
8800 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm
2.90 ft-lb/in
0.25 in; ASTM D256
1.98 J/cm
3.70 ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature -40.0 - 176 °C
72.0 µin/in-°F

@Temperature -40.0 - 349 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 82.8 °C
181 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F
Unannealed; ASTM D648
Vicat Softening Point 87.8 °C
190 °F
ASTM D1525
Flammability, UL94 V-0
V-0
0.0590 in
V-0
V-0
0.0980 in
5VA
5VA
0.0980 in.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 177 °C
330 - 350 °F
Middle Barrel Temperature 168 - 185 °C
335 - 365 °F
Front Barrel Temperature 179 - 191 °C
355 - 375 °F
Nozzle Temperature 174 - 185 °C
345 - 365 °F
Melt Temperature 202 °C
395 °F
Aim
Mold Temperature 40.6 - 71.1 °C
105 - 160 °F
Moisture Content <= 0.10 %
<= 0.10 %
Injection Pressure 4.90 - 5.86 MPa
710 - 850 psi
Back Pressure 0.483 - 0.965 MPa
70.0 - 140 psi
Shot Size 40 - 80 %
40 - 80 %
Screw Speed 50 - 90 rpm
50 - 90 rpm
Descriptive Properties Value Comments
Holding Pressure 570 to 710 psi
Injection Rate Slow-Moderate
Users viewing this material also viewed the following: