Polymer Property : Oxygen Transmission Rate = 2.60 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR ..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 C..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B100MP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B100QP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B100ZP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B135MP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B135QP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B135ZP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B73QP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B85QP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well ..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Average value: 40.3 cc/m²/day Grade Count:17
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B73MP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
BASF Capron® B73ZP Nylon 6 (DAM)  (discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Average value: 40.3 cc/m²/day Grade Count:10
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..