Material Notes:
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Volatiles 0.80 %
0.80 %
Extractable
Water Absorption 1.6 %
1.6 %
24 hr.; ISO 62
9.5 %
9.5 %
ISO 62
Moisture Absorption at Equilibrium 0.080 %
0.080 %
ASTM D570
2.7 %
2.7 %
23°C/50% R.H.; ISO 62
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
cc/m2/day (Thickness not reported)
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
cc/m2/day (Thickness not reported)
Viscosity Measurement 3.7
3.7
Relative Viscosity (95% SAV)
3.75
3.75
Relative Viscosity (96% SAV)
3.9
3.9
Relative Viscosity (98% SAV)
135
135
Formic Acid; ASTM D789
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min
220 °C
428 °F
ASTM D3418
Descriptive Properties Value Comments
Additive Unfilled
Color Natural
Commercial Status (March 2007) Active America
FDA 21 CFR 177.1500
Film Extrusion Processable
Impact Modified No
Primary Processing Technique Film Extrusion