Material Notes:
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Water Absorption 1.6 %
1.6 %
24 hr.; ISO 62
9.5 %
9.5 %
ISO 62
Moisture Absorption at Equilibrium 2.7 %
2.7 %
23°C/50% R.H.; ISO 62
Oxygen Transmission Rate 40.3 cc/m²/day
2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm
35.6 cc-mil/100 in²-24hr-atm
cc/m2/day (Thickness not reported)
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm
185 cc-mil/100 in²-24hr-atm
cc/m2/day (Thickness not reported)
Viscosity Measurement 3.0
3.0
Relative Viscosity (96% SAV)
3.1
3.1
Relative Viscosity (95% SAV)
3.2
3.2
Relative Viscosity (98% SAV)
73
73
Formic Acid; ASTM D789
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 80.0 MPa
11600 psi
50 mm/min; ISO 527
80.0 MPa
11600 psi
2 in/min; ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10 K/min
220 °C
428 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Descriptive Properties Value Comments
Additive Unfilled
Color Natural
Commercial Status (March 2007) Active America
FDA 21 CFR 177.1500
Film Extrusion Processable
Impact Modified No
Injection molding Processable
Primary Processing Technique Film Extrusion