Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 19.7 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 500 microns
19.7 mil
Mapal Plastics Maplon Type 3G Polypropylene Sheet
Maplon type “3G” is a single layer highly polished clear sheets, with anti-blocking properties.Main advantages: High clarity and low haze, Easy to convert due to reduced blocking, High dur..
Thickness 500 microns
19.7 mil
Mapal Plastics Maplon Type D Polypropylene Sheet
Main advantages: High clarity and medium haze, High durability, Water and chemical resistance, High heat resistance, Unlimited flex life of integral hinge, Easy to convertMain disadvantages: Low scr..
Thickness 500 microns
19.7 mil
Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet
Maplon Catalog No. L050-C001K0101 is an extremely opaque white sheet. Sheet surface is smoothly embossed with similar finish on both sides..Main advantages: High opacity, High rigidity high thermal ..
Thickness 500 microns
19.7 mil
Standard
GrafTech GRAFIHX® RXS Series Flexible Graphite Heat Transfer Plates
GRAFIHX® RXS Series are heat transfer plates for radiant heating applications made from high thermal conductivity flexible graphite. They are available in rolls and sheets as a replacement for tr..
Thickness 500 - 5000 microns
19.7 - 197 mil
Daikin NEOFLON AC-5820 PFA Coating Powder, White
NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Electrostatic sp..
Thickness 500 - 5000 microns
19.7 - 197 mil
Daikin NEOFLON AC-5830 PFA Coating Powder, Gray
NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.Info..
Thickness 500 - 5000 microns
19.7 - 197 mil
Daikin NEOFLON NC-1810 FEP Coating Powder, White
NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In..
Thickness 500 - 5000 microns
19.7 - 197 mil
Daikin NEOFLON NC-1830 FEP Coating Powder, Gray
NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In..
Thickness 500 microns
19.7 mil
laminate layer thickness
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..
Thickness 500 microns
19.7 mil
laminate layer thickness
Bond Laminates TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..
Thickness 500 microns
19.7 mil
laminate layer thickness
Bond Laminates TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Within the TEPEX® composite laminate, PP is a resin known for its good hardness, stiffness, abrasion resistance and chemical resistance.Typical application environments are within automotive applic..
Thickness 500 - 2000 microns
19.7 - 78.7 mil
Beijing Evergrow Resources Activated Carbon Paper
Features:good strengthgood flexilitygood durabilityLow air resistanceeasy for mechanical processingApplications:Air purificationWater purificationInformation provided by Beijing Evergrow Resources.