Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 12.7 - 5000 microns | 0.500 - 197 mil | Average value: 1040 microns Grade Count:13 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Thickness | 500 - 5000 microns | 19.7 - 197 mil | |
Daikin NEOFLON AC-5820 PFA Coating Powder, White NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Electrostatic sp.. |
|||
Thickness | 500 - 5000 microns | 19.7 - 197 mil | |
Daikin NEOFLON AC-5830 PFA Coating Powder, Gray NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.Info.. |
|||
Thickness | 500 - 5000 microns | 19.7 - 197 mil | |
Daikin NEOFLON NC-1810 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Thickness | 500 - 5000 microns | 19.7 - 197 mil | |
Daikin NEOFLON NC-1830 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Thickness | 4500 - 5000 microns | 177 - 197 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 4500 - 5000 microns | 177 - 197 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 4500 - 5000 microns | 177 - 197 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 4500 - 5000 microns | 177 - 197 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 4500 - 5000 microns | 177 - 197 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 4500 - 5000 microns | 177 - 197 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1.5 mm Molded Thickness) AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |