Physical Properties Metric English Comments
Thickness 400 - 2000 microns
15.7 - 78.7 mil
Corning Antimicrobial Gorilla® Glass Touch Screen Glass
Antimicrobial Corning® Gorilla® Glass is an antimicrobial cover glass with EPA registration as a treated article. It combines the benefits of Corning® Gorilla® Glass technology, including durabi..
Thickness 400 - 2000 microns
15.7 - 78.7 mil
Corning Gorilla® Glass 3 Touch Screen Glass with NDR
Gorilla® Glass 3 with Native Damage Resistance™ (NDR) is an alkali-aluminosilicate thin sheet glass that is better able to survive the real-world events that most commonly cause glass failure. Wit..
Thickness 550 - 2000 microns
21.7 - 78.7 mil
Corning Large Cover Gorilla® Glass Touch Screen Glass
Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C..
Thickness 500 - 2000 microns
19.7 - 78.7 mil
Beijing Evergrow Resources Activated Carbon Paper
Features:good strengthgood flexilitygood durabilityLow air resistanceeasy for mechanical processingApplications:Air purificationWater purificationInformation provided by Beijing Evergrow Resources.