Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 178 microns | 7.00 mil | Thermal Conductor Thickness |
Parker Chomerics T-Wing™ Heat Spreader Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of.. |
|||
Thickness | 178 - 1520 microns | 7.00 - 60.0 mil | |
Alcoa KAMA 3210 Hi-Gloss Coextruded High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Thickness | 178 microns | 7.00 mil | Nominal |
DuPont™ Nomex® 410 Paper, 7 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 178 microns | 7.00 mil | Nominal |
DuPont™ Nomex® 414 Paper, 7 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 178 microns | 7.00 mil | Nominal |
DuPont™ Nomex® E56 Paper, 7 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 18146R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7048 Screen Printable Extended Life Vinyl Performance Label Products 3M™ Screen Printable Extended Life Vinyl Performance Label Products are high performance materials that offer good conformability and moisture resistance. These vinyl label stocks utilize 3M™ Adhe.. |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon 48366X007 0.007" (0.178 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Thickness | 178 microns | 7.00 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 55869R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 56596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon 66211A007 0.007" (0.178 mm) Uncured Silicone Rubber Monofilament Polyester Fabric Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Monofilament Polyester Fabric Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represent.. |
|||
Thickness | 178 - 254 microns | 7.00 - 10.0 mil | Overall |
Arlon 910-10RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM035 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM045 Clear Polyester Label Product 3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FP012615 White Polyester Label Products ion 3M™ White Polypropylene Label Products are glossy white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV065 Semi-Rigid White Vinyl Label Product 3M™ Semi-Rigid White Vinyl Label Products are white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clarity general.. |
|||
Thickness | 178 microns | 7.00 mil | Facestock |
3M FVS12S Static Cling Label Materials 3M™ Static Cling Label Materials are highly plasticized vinyl label materials available in white or clear that adhere to most clean smooth surfaces such as glass, painted metal, and most smooth pla.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-14 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-81 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7027 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7052W Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™ Adhesive P140.. |
|||
Thickness | 178 microns | 7.00 mil | Side 1 |
Arlon 51224R015P 0.015" Semi-cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and shou.. |
|||
Thickness | 178 microns | 7.00 mil | Side 1 |
Arlon 51344R015 0.015" (0.381 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to .. |
|||
Thickness | 178 microns | 7.00 mil | Polyester |
3M 7961MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM041909 White Polyester Label Products 3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which .. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM095 Indoor UL Recognized Matte Silver Polyester Label Product 3M™ Indoor UL Recognized Matte Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 178 microns | 7.00 mil | |
3M Scotch® Super 33+™ Vinyl Electrical Tape Scotch® Super 33+™ Vinyl Electrical Tape is a premium grade, 7 mil thick, all-weather vinyl-insulating tape. It is designed to perform continuously in ambient temperatures up to 105°C. The tape i.. |
|||
Thickness | 178 microns | 7.00 mil | substrate; Arlon SQA-TMS-003 |
Arlon R37881R015 Silicone Rubber/Fiberglass Interleave: 1.5 mil PE; Side 1: uncured silicone rubber; Substrate: 1528 fiberglass; Side 2: uncured silicone rubber; Interleave: 1.5 mil PE |