Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Evazote® EV45CN Conductive Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Cell Length | 0.250 - 0.600 mm | 0.00984 - 0.0236 in | |
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Plastazote® LD15FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 - 0.600 mm | 0.0118 - 0.0236 in | |
Zotefoams Plastazote® LD30 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.250 - 0.600 mm | 0.00984 - 0.0236 in | |
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.250 - 0.600 mm | 0.00984 - 0.0236 in | |
Zotefoams Plastazote® LD45 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Plastazote® LD15FMSV Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.250 - 0.600 mm | 0.00984 - 0.0236 in | |
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Plastazote® MP15 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Plastazote® MP15FR Metallocene Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.200 - 0.600 mm | 0.00787 - 0.0236 in | |
Zotefoams Plastazote® LD15 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |