Polymer Property : Melt Flow = 60.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.00 - 60.0 g/10 min
4.00 - 60.0 g/10 min
Average value: 23.0 g/10 min Grade Count:41
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Melt Flow 6.00 - 60.0 g/10 min
6.00 - 60.0 g/10 min
Average value: 24.2 g/10 min Grade Count:13
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Melt Flow 6.00 - 60.0 g/10 min
6.00 - 60.0 g/10 min
Average value: 15.6 g/10 min Grade Count:35
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Melt Flow 5.00 - 60.0 g/10 min
5.00 - 60.0 g/10 min
Average value: 19.3 g/10 min Grade Count:15
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Melt Flow 1.90 - 60.0 g/10 min
1.90 - 60.0 g/10 min
Average value: 14.5 g/10 min Grade Count:169
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Melt Flow 0.100 - 60.0 g/10 min
0.100 - 60.0 g/10 min
Average value: 15.7 g/10 min Grade Count:39
Overview of materials for Cyclo Olefin Polymer
This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria..
Melt Flow 3.00 - 60.0 g/10 min
3.00 - 60.0 g/10 min
Average value: 25.9 g/10 min Grade Count:10
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Melt Flow 1.00 - 60.0 g/10 min
1.00 - 60.0 g/10 min
Average value: 16.8 g/10 min Grade Count:15
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Compounding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Compounding Grade". Each property range of values reported is minimu..
Melt Flow 0.600 - 60.0 g/10 min
0.600 - 60.0 g/10 min
Average value: 14.5 g/10 min Grade Count:107
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..
Melt Flow 0.120 - 60.0 g/10 min
0.120 - 60.0 g/10 min
Average value: 2.02 g/10 min Grade Count:309
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..