Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 30.0 g/10 min | 5.00 - 30.0 g/10 min | Average value: 11.6 g/10 min Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Melt Flow | 5.00 - 9.00 g/10 min | 5.00 - 9.00 g/10 min | Average value: 7.92 g/10 min Grade Count:6 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Flow | 5.00 - 17.0 g/10 min | 5.00 - 17.0 g/10 min | Average value: 9.67 g/10 min Grade Count:9 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Melt Flow | 5.00 - 60.0 g/10 min | 5.00 - 60.0 g/10 min | Average value: 19.3 g/10 min Grade Count:15 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1061 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 9000 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1702B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1888 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1907E CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2253 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 1.00 kg, Temperature 235 °C |
5.00 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Teknor Apex Chemlon® 340G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 8313 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1227A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2455 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2745 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2860M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 190 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB006LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Uses: Film Forms: Pellets Processing Method: Blow Moldi.. |
|||
Melt Flow | 5.00 g/10 min @Load 21.6 kg, Temperature 200 °C |
5.00 g/10 min @Load 47.6 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2666 Acrylonitrile Butadiene Styrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (200000 ppm) Uses: Sheet Forms: Pellets Processing Method: Injection Molding; Sheet ExtrusionI.. |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1781 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2363H Thermoplastic Elastomer Availability: North America Uses: Flooring; Furniture; General Purpose; Grommets; Textile Applications; Wire and Cable Applications Forms: Pellets Processing Method: Extrusion; Injection Molding In.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2439D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2420A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU603 ABS Heat Resistant High Impact, High RigidityInformation provided by Bhansali |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Melt Flow | 5.00 - 50.0 g/10 min | 5.00 - 50.0 g/10 min | Average value: 22.7 g/10 min Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Melt Flow | 5.00 - 20.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 20.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW011LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 - 21.0 g/10 min | 5.00 - 21.0 g/10 min | Average value: 15.0 g/10 min Grade Count:10 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |