Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 400 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
Oxford Polymers PEEK 450-INJ-Black PEEK Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol.. |
|||
Melt Flow | 4.00 - 60.0 g/10 min | 4.00 - 60.0 g/10 min | Average value: 23.0 g/10 min Grade Count:41 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Melt Flow | 4.00 - 130 g/10 min | 4.00 - 130 g/10 min | Average value: 49.8 g/10 min Grade Count:7 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Melt Flow | 4.00 - 130 g/10 min | 4.00 - 130 g/10 min | Average value: 42.8 g/10 min Grade Count:13 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1843L1 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1458 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1473F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1848K Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1848R Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2100 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2100-S-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1595 Thermoplastic Elastomer Features: Nice Silken Feel Uses: Leisure ProductsInformation Provided by Teknor Apex |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1353A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 10.0 kg, Temperature 230 °C |
4.00 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2432F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2830E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-102 BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-7100-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 10.0 kg, Temperature 190 °C |
4.00 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB106LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (450000 ppm) Features: General Purpose Uses: Film Forms: Pellets Processing Method: Blow Moldi.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1210A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 - 48.0 g/10 min | 4.00 - 48.0 g/10 min | Average value: 21.0 g/10 min Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |