Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.90 - 60.0 g/10 min | 1.90 - 60.0 g/10 min | Average value: 14.5 g/10 min Grade Count:169 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Melt Flow | 1.90 - 170 g/10 min | 1.90 - 170 g/10 min | Average value: 26.4 g/10 min Grade Count:23 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Melt Flow | 1.90 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.90 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1190A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 1.90 - 7.90 g/10 min | 1.90 - 7.90 g/10 min | Average value: 3.85 g/10 min Grade Count:6 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |