Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company CP850 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer M. Holland Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company CP850 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact copolymerFast production cycleHigh flowHigh stiffnessApplications: ContainersHousehold goodsThin-walled parts
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
73°F; ASTM D256
Descriptive Properties Value Comments
Forms Pellets
Processing Methods Injection molding