Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 50 - 80 g/10 min | 50 - 80 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Melt Flow | 50 - 80 g/10 min | 50 - 80 g/10 min | 50-80 cm<sup>3</sup>/10 min; Melt Volume Rate |
Huntsman IROGRAN® A 85 P 4944 Ether-Based TPU-For Cable Industry High temperature stabilityInformation provided by Huntsman |
|||
Melt Flow | 50 - 80 g/10 min | 50 - 80 g/10 min | Melt Volume Rate (cm³/10 min) |
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext.. |