Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HIPS7240 is a very high impact polystyrene used in the extrusion industry. The good melt strength of this grade makes it particularly suitable for deep-draw thermoforming. HIPS 7240 is available in white color.Applications: extrusion, coextrusion, containers, thermoformingInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Moisture Absorption <= 0.100 %
<= 0.100 %
ASTM D570
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.0 MPa
2900 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 55 %
55 %
ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ASTM D638
Flexural Modulus 1.75 GPa
254 ksi
ASTM D790
Izod Impact, Notched (ISO) 8.50 kJ/m²
4.04 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Vicat Softening Point >= 94.0 °C
>= 201 °F
ASTM D1525