Material Notes:
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Melt Flow 27 g/10 min
27 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 63.5 MPa
9210 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 93.01 MPa
13490 psi
ASTM D790
Flexural Modulus 2.670 GPa
387.2 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F